Tailoring the electrode-electrolyte interface of Solid Oxide Fuel Cells (SOFC) by laser micro-patterning to improve their electrochemical performance
Cathode activation polarisation is one of the main contributions to the losses of a Solid Oxide Fuel Cell. To reduce this loss we use a pulsed laser to modify the surface of yttria stabilized zirconia (YSZ) electrolytes to make a corrugated micro-patterning in the mesoscale. The beam of the laser so...
| Authors: | , , , |
|---|---|
| Format: | article |
| Status: | Versión aceptada para publicación |
| Publication Date: | 2017 |
| Country: | España |
| Institution: | Consejo Superior de Investigaciones Científicas (CSIC) |
| Repository: | DIGITAL.CSIC. Repositorio Institucional del CSIC |
| OAI Identifier: | oai:digital.csic.es:10261/182422 |
| Online Access: | http://hdl.handle.net/10261/182422 |
| Access Level: | Open access |
| Keyword: | SOFC Laser machining Corrugated surface Electrode polarisation Cathode activation Electrode/electrolyte interface |
| Summary: | Cathode activation polarisation is one of the main contributions to the losses of a Solid Oxide Fuel Cell. To reduce this loss we use a pulsed laser to modify the surface of yttria stabilized zirconia (YSZ) electrolytes to make a corrugated micro-patterning in the mesoscale. The beam of the laser source, 5 ns pulse width and emitting at λ = 532 nm (green region), is computer-controlled to engrave the selected micro-pattern on the electrolyte surface. Several laser scanning procedures and geometries have been tested. Finally, we engrave a square array with 28 μm of lattice parameter and 7 μm in depth on YSZ plates. With these plates we prepare LSM-YSZ/YSZ/LSM-YSZ symmetrical cells (LSM: La1-xSrxMnO3) and determine their activation polarisation by Electrochemical Impedance Spectroscopy (EIS). To get good electrode-electrolyte contact after sintering it is necessary to use pressure-assisted sintering with low loads (about 5 kPa), which do not modify the electrode microstructure. The decrease in polarisation with respect to an unprocessed cell is about 30%. EIS analysis confirms that the reason for this decrease is an improvement in the activation processes at the electrode-electrolyte interface. |
|---|