Preparation of ZnFe2O4/ZnO composite: Effect of operational parameters for photocatalytic degradation of dyes under UV and visible illumination

An ZnFe2O4/ZnO composite catalyst was prepared by solution combustion method. In this study, one nominal molar percentage of iron was used in the synthesis, corresponding to 20 % molar relative to ZnO. The samples were characterized by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS),...

Descripción completa

Detalles Bibliográficos
Autores: Zouhier, Morad, Tanji, Karim, Navío, José Antonio, Hidalgo, M. C., Jaramillo-Páez, César, Kherbeche, Abdelhak
Tipo de recurso: artículo
Estado:Versión aceptada para publicación
Fecha de publicación:2020
País:España
Institución:Consejo Superior de Investigaciones Científicas (CSIC)
Repositorio:DIGITAL.CSIC. Repositorio Institucional del CSIC
OAI Identifier:oai:digital.csic.es:10261/400800
Acceso en línea:http://hdl.handle.net/10261/400800
https://api.elsevier.com/content/abstract/scopus_id/85076539209
Access Level:acceso abierto
Palabra clave:Zinc oxide
Iron doped ZnO
Methylene blue
Photocatalysis
Remazol brilliant blue
ZnFe2O4
Descripción
Sumario:An ZnFe2O4/ZnO composite catalyst was prepared by solution combustion method. In this study, one nominal molar percentage of iron was used in the synthesis, corresponding to 20 % molar relative to ZnO. The samples were characterized by X-ray diffraction (XRD), X-ray photoelectron spectroscopy (XPS), X-ray Fluorescence (XRF), Scanning Electronic Microscopy (SEM), Transmission Electronic Microscopy (TEM) and Ultraviolet-visible (UV–vis) diffuse spectroscopy (DRS). The photocatalytic activities of the catalysts were investigated based on the degradation of two dyes, methylene blue (MB) and remazol brilliant blue (RBB), in aqueous solution under both UV and visible light illumination respectively. It was found that the composite had a good photocatalytic activity at basic pH by using 1 g/L of catalyst under UV illumination for both MB and RBB. Under visible illumination, while pristine ZnO showed no activity, the composite exhibited an excellent visible efficiency, reaching up to an 80 % conversion of the initial dye concentrations in 2 h. The enhancement of the visible photocatalytic activity of Fe/ZnO sample with respect to pristine ZnO is attributed to the formation of ZnFe2O4 coupled with ZnO, having a narrow band gap value that contributes to the absorption of visible photons with an improved separation path for the photo-generated carriers.