Dip-coating deposition of resistive BiVO4 thin film and evaluation of their photoelectrochemical parameters under distinct sources illumination

Resistive monoclinic bismuth vanadate (BiVO4) nanocrystals in the form of thin films were obtained by the solution combustion synthesis coupled with the dip-coating deposition process. The structure, morphology, and optical properties of BiVO4 nanocrystals were characterized by means of x-ray diffra...

Descripción completa

Detalles Bibliográficos
Autores: da Silva, M. R. [UNESP], Scalvi, L. V.A. [UNESP], Neto, V. S.L., Dall’Antonia, L. H.
Tipo de recurso: artículo
Estado:Versión publicada
Fecha de publicación:2016
País:Brasil
Institución:Universidade Estadual Paulista (UNESP)
Repositorio:Repositório Institucional da UNESP
Idioma:inglés
OAI Identifier:oai:repositorio.unesp.br:11449/168698
Acceso en línea:http://dx.doi.org/10.1007/s10008-016-3166-y
http://hdl.handle.net/11449/168698
Access Level:acceso abierto
Palabra clave:BiVO4
Dichroic lamp
InGaN LED
Resistive
Thin film
Descripción
Sumario:Resistive monoclinic bismuth vanadate (BiVO4) nanocrystals in the form of thin films were obtained by the solution combustion synthesis coupled with the dip-coating deposition process. The structure, morphology, and optical properties of BiVO4 nanocrystals were characterized by means of x-ray diffraction (XRD), scanning electron microscopy (SEM), and UV-Vis spectroscopy. The photoelectrochemical properties were obtained by cyclic voltammetry and chronoamperometry techniques in potassium chloride (KCl) electrolyte solution under distinct visible light sources irradiation condition. Under blue InGaN light emitting diode (LED) irradiation, the electrode has a better efficiency, faster response time (260 ms), and faster decay time (65 ms), when compared with the irradiation by dichroic lamp. Besides, the photocurrent density (jph) is approximately 39 times higher than jph obtained under dichroic lamp. The performance analysis based on the methylene blue degradation reaction has shown that the BiVO4 material has higher electroactivity under InGaN LED irradiation condition, with estimated kobs value of 200 à  10−4 min−1, which is a little higher than the value obtained with dichroic lamp illumination. In the dark condition, the BiVO4 presented much lower photocatalytic activity.