Role of exciton diffusion in the efficiency of Mn dopant emission in two-dimensional perovskites

Two-dimensional (2D) metal-halide perovskites have promising characteristics for optoelectronic applications. By incorporating Mn2+ ions into the perovskite structure, improved photoluminescence quantum yield can be achieved. This has been attributed to the formation of defect states that act as eff...

Descripción completa

Detalles Bibliográficos
Autores: Magdaleno de Benito, Alvaro Javier, Kshirsagar, Anuraj S., Meléndez Schofield, Marc, Kuruppu, Udara M., Suurmond, Jesse J., Cutler, Mercy M., Frising, Michel, Seitz, Michael, Delgado Buscalioni, Rafael, Gangishetty, Mahesh K., Prins, Ferry
Tipo de recurso: artículo
Fecha de publicación:2024
País:España
Institución:Universidad Autónoma de Madrid
Repositorio:Biblos-e Archivo. Repositorio Institucional de la UAM
Idioma:inglés
OAI Identifier:oai:repositorio.uam.es:10486/716509
Acceso en línea:http://hdl.handle.net/10486/716509
https://dx.doi.org/10.1021/acsnanoscienceau.4c00047
Access Level:acceso abierto
Palabra clave:2D Perovskites
Mn Doping
Exciton Diffusion
Transient Microscopy
Carrier Dynamics
Física
Descripción
Sumario:Two-dimensional (2D) metal-halide perovskites have promising characteristics for optoelectronic applications. By incorporating Mn2+ ions into the perovskite structure, improved photoluminescence quantum yield can be achieved. This has been attributed to the formation of defect states that act as efficient recombination centers. Here, we make use of transient photoluminescence microscopy to characterize important material parameters of Mn2+-doped 2D perovskites with different doping levels. From these measurements, we visualize the importance of exciton transport as an intermediate step in the excitation of Mn2+. We model the spatiotemporal dynamics of the excited states to extract the diffusion constant and the transfer rate of the excitations to the Mn dopant sites. Interestingly, from these models, we find that the average distance an exciton needs to travel before transferring to a Mn site is significantly larger than expected from the Mn concentration obtained from elemental analysis. These insights are critical from a device design perspective