Correction of secondary fluorescence across phase boundaries in electron probe microanalysis of mineral inclusions

One of the limiting factors for the analysis of minor elements in multiphase materials by electron probe microanalysis is the effect of secondary fluorescence (SF), which is not accounted for by matrix corrections. Although the apparent concentration due to SF can be calculated numerically or measur...

ver descrição completa

Detalhes bibliográficos
Autores: Llovet, Xavier, Proenza, Joaquín A., Pujol-Solà, Núria, Farré-de-Pablo, Júlia, Campeny, Marc
Tipo de documento: artigo
Estado:Versión aceptada para publicación
Data de publicação:2020
País:España
Recursos:Varias* (Consorci de Biblioteques Universitáries de Catalunya, Centre de Serveis Científics i Acadèmics de Catalunya)
Repositório:Recercat. Dipósit de la Recerca de Catalunya
OAI Identifier:oai:recercat.cat:2072/376765
Acesso em linha:http://hdl.handle.net/2072/376765
https://doi.org/10.1017/S1431927620024393
Access Level:Acceso aberto
Palavra-chave:Microscòpia de fluorescència
Silicats
Cromita
Serpentinita
Quars
549
Descrição
Resumo:One of the limiting factors for the analysis of minor elements in multiphase materials by electron probe microanalysis is the effect of secondary fluorescence (SF), which is not accounted for by matrix corrections. Although the apparent concentration due to SF can be calculated numerically or measured experimentally, detailed investigations of this effect for fine-grained materials are scarce. In this work, we use the Monte Carlo simulation program PENEPMA to examine and correct the effect of SF affecting micron-sized mineral inclusions hosted by other minerals. A concentration profile across an olivine [(Mg,Fe)2SiO4] inclusion in chromite (Fe2+Cr2O4) is measured and used to assess the reliability of calculations, where different boundary geometries are examined. Three application examples are presented, which include the determination of Cr in olivine and serpentine [Mg3Si2O5(OH)4] inclusions hosted by chromite and of Fe in quartz (SiO2) inclusions hosted by almandine garnet (Fe3Al2Si3O12). Our results show that neglecting SF leads to concentrations that are overestimated by ~0.1–0.8 wt%, depending on inclusion size. In addition, assuming a straight boundary yields to an underestimation of SF effects by a factor of ~2–4. Because its long-range nature, SF severely compromises trace element analyses even for phases as large as 1 mm in size.