Effects of synthetic conditions on the structural, stability and ion conducting properties of Li0.30(La0.50Ln0.50)0.567TiO3 (Ln= La, Pr, Nd) solid electrolytes for rechargeable lithium batteries

The structure, thermal stability, morphology and ion conductivity of titanium perovskites with the general formula Li3xLn2/3−xTiO3 (Ln = rare earth element; 3x= 0.30) are studied in the context of their possible use as solid electrolyte materials for lithium ion batteries. Materials are prepared by...

Descripción completa

Detalles Bibliográficos
Autores: Vidal García, Karmele, Ortega San Martín, Luis, Larrañaga Varga, Aitor, Merino Rubio, Rosa Isabel, Orera Utrilla, Alodia, Arriortua Marcaida, María Isabel
Tipo de recurso: artículo
Fecha de publicación:2014
País:España
Institución:Universidad del País Vasco
Repositorio:Addi. Archivo Digital para la Docencia y la Investigación
OAI Identifier:oai:addi.ehu.eus:10810/18324
Acceso en línea:http://hdl.handle.net/10810/18324
Access Level:acceso abierto
Palabra clave:lithium-ion conductor
perovskite structure
combustion synthesis
lithium ion batteries
Descripción
Sumario:The structure, thermal stability, morphology and ion conductivity of titanium perovskites with the general formula Li3xLn2/3−xTiO3 (Ln = rare earth element; 3x= 0.30) are studied in the context of their possible use as solid electrolyte materials for lithium ion batteries. Materials are prepared by a glycine-nitrate method using different sintering treatments, with a cation-disorder-induced structural transition from tetragonal to cubic symmetry, detected as quenching temperature increases. SEM images show that the average grain size increases with increasing sintering temperature and time. Slightly higher bulk conductivity values have been observed for quenched samples sintered at high temperature. Bulk conductivity decreases with the lanthanide ion size. A slight conductivity enhancement, always limited by grain boundaries, is observed for longer sintering times. TDX measurements of the electrolyte/cathode mixtures also show a good stability of the electrolytes in the temperature range of 30-1100ºC.