The use of spent glauconite in lightweight aggregate production
The presented work has shown an application of spent glauconite bed after purification of wastewater for production of lightweight expanded clay aggregates. Sewage, from which it was removed Zn ions, came from technological line (zincworks) of Communication Equipment Factory „PZL” Świdnik. Spent gla...
| Autores: | , |
|---|---|
| Tipo de recurso: | artículo |
| Fecha de publicación: | 2011 |
| País: | España |
| Institución: | Consejo Superior de Investigaciones Científicas (CSIC) |
| Repositorio: | DIGITAL.CSIC. Repositorio Institucional del CSIC |
| OAI Identifier: | oai:digital.csic.es:10261/41754 |
| Acceso en línea: | http://hdl.handle.net/10261/41754 |
| Access Level: | acceso abierto |
| Palabra clave: | Glauconite Pickle wastewater |
| Sumario: | The presented work has shown an application of spent glauconite bed after purification of wastewater for production of lightweight expanded clay aggregates. Sewage, from which it was removed Zn ions, came from technological line (zincworks) of Communication Equipment Factory „PZL” Świdnik. Spent glauconite bed was used as an additive in lightweight aggregate production which was obtained using plastic method by sintering, at temperature 1140ºC and 1200 ºC, of spent glauconite amouts 10, 15, 20 and 25% wt. with clays from open-cast mine „Budy Mszczonowskie”. The presence of the mineral improves sinter texture, increases porosity and contributes to formation of glassy layer on the surface of the aggregates. Tests of zinc elution from lightweight of aggregate samples has shown very low mobility of zinc ions. Content of zinc in water extracts obtained from lightweight of aggregate is definitely lower than zinc concentration permitted for sewage discharge to water or soil, means that spent material is not offensive for the environment as it can be used as a high quality building product. |
|---|