Evaluation of synthesis conditions for plastic scintillation foils used to measure alpha- and beta-emitting radionuclides

Plastic scintillation foils of polystyrene and polycarbonate with a thickness between 45 and 200 μm, have been produced using the solvent evaporation method. PSfoils presented a reproducible thickness (10-20%). PSfoils were characterized by the measurement of 36Cl or 241Am. For 36Cl spectrum is loca...

ver descrição completa

Detalhes bibliográficos
Autores: Merín, R., Tarancón Sanz, Alex, Mitev, K., Georgiev, S., Bagán Navarro, Héctor, García Martínez, José Francisco
Formato: artículo
Estado:Versión aceptada para publicación
Fecha de publicación:2018
País:España
Recursos:Varias* (Consorci de Biblioteques Universitáries de Catalunya, Centre de Serveis Científics i Acadèmics de Catalunya)
Repositorio:Recercat. Dipósit de la Recerca de Catalunya
OAI Identifier:oai:recercat.cat:2445/130019
Acesso em linha:https://hdl.handle.net/2445/130019
Access Level:acceso abierto
Palavra-chave:Anàlisi radioquímica
Radioactivitat
Radiochemical analysis
Radioactivity
Descrição
Resumo:Plastic scintillation foils of polystyrene and polycarbonate with a thickness between 45 and 200 μm, have been produced using the solvent evaporation method. PSfoils presented a reproducible thickness (10-20%). PSfoils were characterized by the measurement of 36Cl or 241Am. For 36Cl spectrum is located at medium energies since not all energy is deposited in the scintillator and not all betas interact with the foils. For 241Am the efficiency values are very high and spectrum is a sharp peak located at high energies. 222Rn absorption (LD and K) and desorption capacities of the PSfoils have been also evaluated.