Migration of antimony from polyethylene terephthalate used in mineral water bottles.
The influence of storage time and temperature on Sb migration from PET bottles into mineral water was studied in short-term tests lasting up to 15 days and long-term studies lasting up to 220 days. Samples purchased were stored in three different coloured bottles: clear (CL), light blue (LB) and dar...
| Autores: | , , , |
|---|---|
| Tipo de recurso: | artículo |
| Estado: | Versión aceptada para publicación |
| Fecha de publicación: | 2014 |
| País: | España |
| Institución: | Varias* (Consorci de Biblioteques Universitáries de Catalunya, Centre de Serveis Científics i Acadèmics de Catalunya) |
| Repositorio: | Recercat. Dipósit de la Recerca de Catalunya |
| OAI Identifier: | oai:recercat.cat:2445/57563 |
| Acceso en línea: | https://hdl.handle.net/2445/57563 |
| Access Level: | acceso abierto |
| Palabra clave: | Aigües minerals Tereftalat de polietilè Envasos Química analítica Semimetalls Contaminació de l'aigua Mineral waters Polyethylene terephthalate Containers Analytical chemistry Semimetals Water pollution |
| Sumario: | The influence of storage time and temperature on Sb migration from PET bottles into mineral water was studied in short-term tests lasting up to 15 days and long-term studies lasting up to 220 days. Samples purchased were stored in three different coloured bottles: clear (CL), light blue (LB) and dark blue (DB). Sb migration was assayed by HG-AFS for total determination and HPLC-ICP-MS for speciation analysis. Migration studies showed that waters stored at 4 and 20 oC were not subject to Sb migration. At 40 oC there was a significant increase in Sb concentration, although the maximum limit established by the European Union (5.0 ug/L) was not exceeded, whereas at 60 oC samples were subject to considerable Sb migration after 30 days of storage. In this case, the maximum limit established by the European Union was exceeded and both Sb (V) and Sb (III) were detected. |
|---|