All-d-metal Ni(Co)-Mn(X)-Ti (X = Fe or Cr) Heusler Alloys: Enhanced Magnetocaloric Effect for Moderate Magnetic Fields

All-d-metal Ni(Co)-Mn-Ti Heusler alloys show high magnetocaloric/barocaloric effects ascribed to the occurrence of a martensitic transformation together with excellent mechanical properties. However, high magnetic fields are needed to fully drive the transformation and to obtain their maximum respon...

Descripción completa

Detalles Bibliográficos
Autores: Khan, Aun N., Moreno Ramírez, Luis Miguel, Díaz García, Álvaro, Law, Jia Yan, Franco García, Victorino
Tipo de recurso: artículo
Estado:Versión publicada
Fecha de publicación:2023
País:España
Institución:Universidad de Sevilla (US)
Repositorio:idUS. Depósito de Investigación de la Universidad de Sevilla
OAI Identifier:oai:idus.us.es:11441/152180
Acceso en línea:https://hdl.handle.net/11441/152180
https://doi.org/10.1016/j.jallcom.2022.167559
Access Level:acceso abierto
Palabra clave:All-d-metal Heusler alloys
Magnetocaloric effect
Magnetostructural transition
Ni(Co)-Mn-Ti
Descripción
Sumario:All-d-metal Ni(Co)-Mn-Ti Heusler alloys show high magnetocaloric/barocaloric effects ascribed to the occurrence of a martensitic transformation together with excellent mechanical properties. However, high magnetic fields are needed to fully drive the transformation and to obtain their maximum responses. To further tune the martensitic transition and the associated magnetocaloric response, we systematically investigate the role of partial Mn substitution by Fe or Cr on the parent composition Ni36Co14Mn35Ti15. On the one hand, Cr doping increases the entropy change of the transformation but causes a tighter overlap of both martensitic and Curie transitions. This significantly reduces the magnetization difference between austenite and martensite and, consequently, strongly decreases the magnetocaloric response. On the other hand, Fe doping reduces the entropy change of the transformation and separates both martensitic and Curie transitions while keeping the magnetization difference among both phases. These two combined features reduce the magnetic field needed to completely drive the martensitic transformation and leads to higher and broader isothermal entropy change peaks for moderate magnetic field changes, reaching up to 25% enhancement for 2 T when compared to the undoped alloy.