Thermal and oxidation stability of TixW1−x diffusion barriers investigated by soft and hard x-ray photoelectron spectroscopy

The binary alloy of titanium-tungsten (TiW) is an established diffusion barrier in high-power semiconductor devices, owing to its ability to suppress the diffusion of copper from the metallization scheme into the surrounding silicon substructure. However, little is known about the response of TiW to...

ver descrição completa

Detalhes bibliográficos
Autores: Kalha, Curran, Fernando, Nathalie Kanchena, Berens, Judith, Gutierrez Moreno, Jose Julio, Mohr, Stephan|||0000-0003-2510-5805
Formato: artículo
Fecha de publicación:2021
País:España
Recursos:Universitat Politècnica de Catalunya (UPC)
Repositorio:UPCommons. Portal del coneixement obert de la UPC
Idioma:inglés
OAI Identifier:oai:upcommons.upc.edu:2117/345840
Acesso em linha:https://hdl.handle.net/2117/345840
https://dx.doi.org/10.1063/5.0048304
Access Level:acceso abierto
Palavra-chave:Alloys
X-ray photoelectron spectroscopy.
Titanium alloys
Annealing
X-ray photoelectron spectroscopy
Depth profiling techniques
Metallization process
Microfabrication
Density functional theory
Diffusion barriers
Semiconductor devices
Semiconductors
Àrees temàtiques de la UPC::Física
Descrição
Resumo:The binary alloy of titanium-tungsten (TiW) is an established diffusion barrier in high-power semiconductor devices, owing to its ability to suppress the diffusion of copper from the metallization scheme into the surrounding silicon substructure. However, little is known about the response of TiW to high-temperature events or its behavior when exposed to air. Here, a combined soft and hard x-ray photoelectron spectroscopy (XPS) characterization approach is used to study the influence of post-deposition annealing and titanium concentration on the oxidation behavior of a 300 nm-thick TiW film. The combination of both XPS techniques allows for the assessment of the chemical state and elemental composition across the surface and bulk of the TiW layer. The findings show that in response to high-temperature annealing, titanium segregates out of the mixed metal system and upwardly migrates, accumulating at the TiW/air interface. Titanium shows remarkably rapid diffusion under relatively short annealing timescales, and the extent of titanium surface enrichment is increased through longer annealing periods or by increasing the bulk titanium concentration. Surface titanium enrichment enhances the extent of oxidation both at the surface and in the bulk of the alloy due to the strong gettering ability of titanium. Quantification of the soft x-ray photoelectron spectra highlights the formation of three tungsten oxidation environments, attributed to WO2, WO3, and a WO3 oxide coordinated with a titanium environment. This combinatorial characterization approach provides valuable insights into the thermal and oxidation stability of TiW alloys from two depth perspectives, aiding the development of future device technologies.