Compatibilization and Characterization of Polylactide and Biopolyethylene Binary Blends by Non-Reactive and Reactive Compatibilization Approaches

[EN] In this study, different compatibilizing agents were used to analyze their influence on immiscible blends of polylactide (PLA) and biobased high-density polyethylene (bioPE) 80/20 (wt/wt). The compatibilizing agents used were polyethylene vinyl acetate (EVA) with a content of 33% of vinyl aceta...

Descripción completa

Detalles Bibliográficos
Autores: Ferri, J.M|||0000-0002-1269-4973, Garcia-Garcia, Daniel|||0000-0002-2520-0186, E. Rayón|||0000-0002-0653-2046, Samper, María-Dolores|||0000-0002-5102-8412, Balart, Rafael|||0000-0001-5670-7126
Tipo de recurso: artículo
Fecha de publicación:2020
País:España
Institución:Universitat Politècnica de València (UPV)
Repositorio:RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia
Idioma:inglés
OAI Identifier:oai:riunet.upv.es:10251/163181
Acceso en línea:https://riunet.upv.es/handle/10251/163181
Access Level:acceso abierto
Palabra clave:Polylactide
Biopolymers
Blends
Compatibilizing agents
Microscopic techniques
CIENCIA DE LOS MATERIALES E INGENIERIA METALURGICA
09.- Desarrollar infraestructuras resilientes, promover la industrialización inclusiva y sostenible, y fomentar la innovación
12.- Garantizar las pautas de consumo y de producción sostenibles
Descripción
Sumario:[EN] In this study, different compatibilizing agents were used to analyze their influence on immiscible blends of polylactide (PLA) and biobased high-density polyethylene (bioPE) 80/20 (wt/wt). The compatibilizing agents used were polyethylene vinyl acetate (EVA) with a content of 33% of vinyl acetate, polyvinyl alcohol (PVA), and dicumyl peroxide (DPC). The influence of each compatibilizing agent on the mechanical, thermal, and microstructural properties of the PLA-bioPE blend was studied using different microscopic techniques (i.e., field emission electron microscopy (FESEM), transmission electron microscopy (TEM), and atomic force microscopy with PeakForce quantitative nanomechanical mapping (AFM-QNM)). Compatibilized PLA-bioPE blends showed an improvement in the ductile properties, with EVA being the compatibilizer that provided the highest elongation at break and the highest impact-absorbed energy (Charpy test). In addition, it was observed by means of the different microscopic techniques that the typical droplet-like structure is maintained, but the use of compatibilizers decreases the dimensions of the dispersed droplets, leading to improved interfacial adhesion, being more pronounced in the case of the EVA compatibilizer. Furthermore, the incorporation of the compatibilizers caused a very marked decrease in the crystallinity of the immiscible PLA-bioPE blend