Mg2SiO4-MgAl2O4 Directionally Solidified Eutectics: Hardness Dependence Modelled Through an Array of Screw Dislocations

Mg2SiO4-MgAl2O4 eutectic ceramics have been fabricated by means of the laser floating zone (LFZ) technique. The microstructure has revealed as an unusual one at lower growth rate, composed of broken lamellae of MgAl2O4 distributed randomly along one matrix, composed of Mg2SiO4. At higher growth rate...

Descripción completa

Detalles Bibliográficos
Autores: Moshtaghion, Bibi Malmal, Gómez García, Diego, Peña, Jose I.
Tipo de recurso: artículo
Estado:Versión aceptada para publicación
Fecha de publicación:2020
País:España
Institución:Universidad de Sevilla (US)
Repositorio:idUS. Depósito de Investigación de la Universidad de Sevilla
OAI Identifier:oai:idus.us.es:11441/142922
Acceso en línea:https://hdl.handle.net/11441/142922
https://doi.org/10.1016/j.jeurceramsoc.2020.05.015
Access Level:acceso abierto
Palabra clave:Hardness dependence
Lamellar structure
Laser floating zone
Mg2SiO4-MgAl2O4eutectic
Descripción
Sumario:Mg2SiO4-MgAl2O4 eutectic ceramics have been fabricated by means of the laser floating zone (LFZ) technique. The microstructure has revealed as an unusual one at lower growth rate, composed of broken lamellae of MgAl2O4 distributed randomly along one matrix, composed of Mg2SiO4. At higher growth rates, a cell structure with intra-cell lamella structure is dominant. Contrary to most eutectic systems, hardness is not dependent upon the inter-spacing, but it does depend on one characteristic length of lamellae: their perimeter. One simple model based upon the dislocation is proposed, which successfully accounts for such extraordinary hardness law. Accordingly, Mg2SiO4-MgAl2O4 eutectic ceramics fabricated at 50 mm/h growth rate with the smallest MgAl2O4 lamella perimeter favorably showed more elevated hardness (13.4 GPa from Vickers indentation and 15.3 GPa from nanoindentation) and strength (∼430 MPa) than those found in the monolithic Mg2SiO4 matrix.