High-pressure catalytic hydrogenation of renewable succinic acid to 1,4-butanediol for the synthesis of fully bio-based poly(butylene succinate)

The present study puts the circular Bioeconomy Concept into action by synthesizing biodegradable poly(butylene succinate) (PBS) by the polycondensation reaction of renewable succinic acid (SA) and 1,4-butanediol (BDO). To achieve this, SA was first obtained from furfural derived from biomass, which...

Descripción completa

Detalles Bibliográficos
Autores: Flores, Yaiza, Pacheco-Romeralo, Marta, Mboumba, Effie, Alla Bedahnane, Abdelilah|||0000-0001-8417-4937, Lagarón Cabello, José María, Lopez-Granados, Manuel, Martínez de Ilarduya Sáez de Asteasu, Domingo Antxon|||0000-0001-8105-2168, Perret, Noémie, Torres Giner, Sergio
Tipo de recurso: artículo
Fecha de publicación:2025
País:España
Institución:Universitat Politècnica de Catalunya (UPC)
Repositorio:UPCommons. Portal del coneixement obert de la UPC
Idioma:inglés
OAI Identifier:oai:upcommons.upc.edu:2117/438948
Acceso en línea:https://hdl.handle.net/2117/438948
https://dx.doi.org/10.1021/acssuschemeng.4c10409
Access Level:acceso abierto
Palabra clave:Poly(butylene succinate)
PBS
Green chemistry
Bio-based
Synthesis
Characterization
properties
Àrees temàtiques de la UPC::Enginyeria química
Descripción
Sumario:The present study puts the circular Bioeconomy Concept into action by synthesizing biodegradable poly(butylene succinate) (PBS) by the polycondensation reaction of renewable succinic acid (SA) and 1,4-butanediol (BDO). To achieve this, SA was first obtained from furfural derived from biomass, which was gas-phase oxidized to produce maleic acid that was thereafter hydrogenated with a formic acid (FA)-containing water solution. After that, the resultant SA was subjected to catalytic hydrogenation at high pressure to yield BDO. Thus, the polymerization of both renewable monomers was successfully performed in two steps, namely esterification and transesterification, leading to PBS with a similar molecular weight and physical performance to current petrochemical grades commercially available. Finally, the fully bio-based PBS was thermo-compressed into films and originally applied as thermo-sealed bags to package beef meat, successfully achieving food preservation for up to 8 days under refrigeration conditions. Therefore, the resultant biopolyester represents a highly sustainable technical solution in the development of biodegradable food packaging materials, enabling the sourcing of its monomers completely from biomass.