Micro Push-Out Bond Strength of Resin Composite to Dentin in Primary Dentition Using Three Universal Adhesives with Different pH: An In Vitro Study
To evaluate the bond strength of different universal adhesives on deciduous tooth dentine and their relationship with the composition and potential of hydrogen (pH). Methods: An in vitro micro push-out test on 150 samples (n = 50) per group per adhesive, namely, Adhese Universal (ADH; Ivoclar Vivade...
| Autores: | , , , , , , |
|---|---|
| Tipo de recurso: | artículo |
| Fecha de publicación: | 2021 |
| País: | España |
| Institución: | Universidad Europea (UEM) |
| Repositorio: | ABACUS. Repositorio de Producción Científica |
| Idioma: | español |
| OAI Identifier: | oai:abacus.universidadeuropea.com:11268/11991 |
| Acceso en línea: | http://hdl.handle.net/11268/11991 |
| Access Level: | acceso abierto |
| Palabra clave: | Materiales dentales Materiales biocompatibles Cementos dentales Odontología Tecnología médica |
| Sumario: | To evaluate the bond strength of different universal adhesives on deciduous tooth dentine and their relationship with the composition and potential of hydrogen (pH). Methods: An in vitro micro push-out test on 150 samples (n = 50) per group per adhesive, namely, Adhese Universal (ADH; Ivoclar Vivadent), Futurabond U (FUT; Voco GmbH) (Test), and Scotchbond Universal with pre-conditioning (SCO; 3M) (Control), to record bond strength (BS) and type of adhesive failure. Results: The results of the different adhesives (megapascals (MPa)) varied, showing no statistical significance. The corresponding averages are in MPa: ADH, 13.66 ± 2.81; FUT, 14.48 ± 2.88; SCO, 14.98 ± 3.96. Additionally, the frequency of type of failure was as follows: mixed (60.7%), adhesive (27.3%), and cohesive (12%). Conclusions: SCO, with a pH of 2.7, showed greater resistance to fracture, while FUT, with a pH of 2.3 and no pre-conditioning, approached the same values, being a one-step adhesive. No relationship was found between failure and type of adhesive. |
|---|