Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene
Recovery of recycled acrylonitrile-butadiene-styrene (ABS) through mixing with styrene-ethylene/butylene-styrene (SEBS) has been studied in this paper. To simulate recycled ABS, virgin ABS was processed through 5 cycles, at extreme processing temperatures, 220 degrees C and 260 degrees C. The virgin...
| Autores: | , , , |
|---|---|
| Tipo de recurso: | artículo |
| Fecha de publicación: | 2013 |
| País: | España |
| Institución: | Universitat Politècnica de València (UPV) |
| Repositorio: | RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia |
| Idioma: | inglés |
| OAI Identifier: | oai:riunet.upv.es:10251/47988 |
| Acceso en línea: | https://riunet.upv.es/handle/10251/47988 |
| Access Level: | acceso abierto |
| Palabra clave: | Degradation Recovery ABS SEBS Injection Shrinkage CIENCIA DE LOS MATERIALES E INGENIERIA METALURGICA INGENIERIA DE LOS PROCESOS DE FABRICACION |
| id |
ES_49d19cd47aefffc0ea413de07f225f57 |
|---|---|
| oai_identifier_str |
oai:riunet.upv.es:10251/47988 |
| network_acronym_str |
ES |
| network_name_str |
España |
| repository_id_str |
|
| spelling |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrenePeydro, M. A.|||0000-0002-8503-1505Parres, F.|||0000-0002-1083-9526Crespo, J.E|||0000-0003-1372-4289Navarro Vidal, RaúlDegradationRecoveryABSSEBSInjectionShrinkageCIENCIA DE LOS MATERIALES E INGENIERIA METALURGICAINGENIERIA DE LOS PROCESOS DE FABRICACIONRecovery of recycled acrylonitrile-butadiene-styrene (ABS) through mixing with styrene-ethylene/butylene-styrene (SEBS) has been studied in this paper. To simulate recycled ABS, virgin ABS was processed through 5 cycles, at extreme processing temperatures, 220 degrees C and 260 degrees C. The virgin ABS, the virgin SEBS, the recycled ABS and the mixtures were mechanically, thermally and rheologically characterized after the various cycles of reprocessing in order to evaluate their corresponding properties and correlate them with the number of cycles undergone. With these data and using Computer Aided Engineering (CAE) the injection process was simulated by obtaining the optimal injection process parameters. Mixtures were injected at two temperatures in a sensorised mold correlating the shrinkage of the parts with temperature. The results show that tensile strength of ABS remains practically constant as the number of reprocessing cycles increases, while in the material injected with SEBS the tensile strength decreases. Concerning the Charpy notched impact strength; the values of the ABS reprocessed at 220 degrees C remain more or less unchanged, while the values for 260 C show a significant decrease. The adhesion of the SEBS causes, in both cases, an increase in impact strength. DSC techniques enabled us to observe how the glass transition temperature (T-g) remains more or less constant regardless of the number of cycles or the temperature, whereas the crosslinking is much greater in the samples reprocessed at 260 C. Finally, the viscosity decreases with each cycle and this decrease becomes even more noticeable with the addition of SEBS, and also that the parts molded at lower temperatures have less shrinkage. (c) 2013 Elsevier B.V. All rights reserved.We would like to thank the Vice-Directorate of Research, Development and Innovation of the Polytechnic University of Valencia for the help granted to the project: "Ternary systems research applied to polymeric materials for the upgrading of waste styrene", Ref: 20091056 within the program of First Projects of Investigation (PAID 06-09) where this work is framed.ElsevierDepartamento de Ingeniería Mecánica y de Materiales Instituto Universitario de Investigación de Tecnología de los Materiales de la UPVEscuela Politécnica Superior de AlcoyUniversitat Politècnica de ValènciaRepositorio Institucional de la Universitat Politècnica de València Riunet20132013-08-01journal articlehttp://purl.org/coar/resource_type/c_6501VoRhttp://purl.org/coar/version/c_970fb48d4fbd8a85info:eu-repo/semantics/articleapplication/pdfapplication/pdfhttps://riunet.upv.es/handle/10251/47988reponame:RiuNet. Repositorio Institucional de la Universitat Politécnica de Valénciainstname:Universitat Politècnica de València (UPV)InglésengUniversitat Politècnica de València https://doi.org/10.13039/501100004233 PAID-06-09-20091056 Ternary systems research applied to polymeric materials for the upgrading of waste styreneopen accesshttp://purl.org/coar/access_right/c_abf2Reserva de todos los derechoshttp://rightsstatements.org/vocab/InC/1.0/info:eu-repo/semantics/openAccessoai:riunet.upv.es:10251/479882026-06-13T07:49:27Z |
| dc.title.none.fl_str_mv |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene |
| title |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene |
| spellingShingle |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene Peydro, M. A.|||0000-0002-8503-1505 Degradation Recovery ABS SEBS Injection Shrinkage CIENCIA DE LOS MATERIALES E INGENIERIA METALURGICA INGENIERIA DE LOS PROCESOS DE FABRICACION |
| title_short |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene |
| title_full |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene |
| title_fullStr |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene |
| title_full_unstemmed |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene |
| title_sort |
Recovery of recycled acrylonitrile-butadiene-styrene, through mixing with styrene-ethylene/butylene-styrene |
| dc.creator.none.fl_str_mv |
Peydro, M. A.|||0000-0002-8503-1505 Parres, F.|||0000-0002-1083-9526 Crespo, J.E|||0000-0003-1372-4289 Navarro Vidal, Raúl |
| author |
Peydro, M. A.|||0000-0002-8503-1505 |
| author_facet |
Peydro, M. A.|||0000-0002-8503-1505 Parres, F.|||0000-0002-1083-9526 Crespo, J.E|||0000-0003-1372-4289 Navarro Vidal, Raúl |
| author_role |
author |
| author2 |
Parres, F.|||0000-0002-1083-9526 Crespo, J.E|||0000-0003-1372-4289 Navarro Vidal, Raúl |
| author2_role |
author author author |
| dc.contributor.none.fl_str_mv |
Departamento de Ingeniería Mecánica y de Materiales Instituto Universitario de Investigación de Tecnología de los Materiales de la UPV Escuela Politécnica Superior de Alcoy Universitat Politècnica de València Repositorio Institucional de la Universitat Politècnica de València Riunet |
| dc.subject.none.fl_str_mv |
Degradation Recovery ABS SEBS Injection Shrinkage CIENCIA DE LOS MATERIALES E INGENIERIA METALURGICA INGENIERIA DE LOS PROCESOS DE FABRICACION |
| topic |
Degradation Recovery ABS SEBS Injection Shrinkage CIENCIA DE LOS MATERIALES E INGENIERIA METALURGICA INGENIERIA DE LOS PROCESOS DE FABRICACION |
| description |
Recovery of recycled acrylonitrile-butadiene-styrene (ABS) through mixing with styrene-ethylene/butylene-styrene (SEBS) has been studied in this paper. To simulate recycled ABS, virgin ABS was processed through 5 cycles, at extreme processing temperatures, 220 degrees C and 260 degrees C. The virgin ABS, the virgin SEBS, the recycled ABS and the mixtures were mechanically, thermally and rheologically characterized after the various cycles of reprocessing in order to evaluate their corresponding properties and correlate them with the number of cycles undergone. With these data and using Computer Aided Engineering (CAE) the injection process was simulated by obtaining the optimal injection process parameters. Mixtures were injected at two temperatures in a sensorised mold correlating the shrinkage of the parts with temperature. The results show that tensile strength of ABS remains practically constant as the number of reprocessing cycles increases, while in the material injected with SEBS the tensile strength decreases. Concerning the Charpy notched impact strength; the values of the ABS reprocessed at 220 degrees C remain more or less unchanged, while the values for 260 C show a significant decrease. The adhesion of the SEBS causes, in both cases, an increase in impact strength. DSC techniques enabled us to observe how the glass transition temperature (T-g) remains more or less constant regardless of the number of cycles or the temperature, whereas the crosslinking is much greater in the samples reprocessed at 260 C. Finally, the viscosity decreases with each cycle and this decrease becomes even more noticeable with the addition of SEBS, and also that the parts molded at lower temperatures have less shrinkage. (c) 2013 Elsevier B.V. All rights reserved. |
| publishDate |
2013 |
| dc.date.none.fl_str_mv |
2013 2013-08-01 |
| dc.type.none.fl_str_mv |
journal article http://purl.org/coar/resource_type/c_6501 VoR http://purl.org/coar/version/c_970fb48d4fbd8a85 |
| dc.type.openaire.fl_str_mv |
info:eu-repo/semantics/article |
| format |
article |
| dc.identifier.none.fl_str_mv |
https://riunet.upv.es/handle/10251/47988 |
| url |
https://riunet.upv.es/handle/10251/47988 |
| dc.language.none.fl_str_mv |
Inglés eng |
| language_invalid_str_mv |
Inglés |
| language |
eng |
| dc.relation.none.fl_str_mv |
Universitat Politècnica de València https://doi.org/10.13039/501100004233 PAID-06-09-20091056 Ternary systems research applied to polymeric materials for the upgrading of waste styrene |
| dc.rights.none.fl_str_mv |
open access http://purl.org/coar/access_right/c_abf2 Reserva de todos los derechos http://rightsstatements.org/vocab/InC/1.0/ |
| dc.rights.openaire.fl_str_mv |
info:eu-repo/semantics/openAccess |
| rights_invalid_str_mv |
open access http://purl.org/coar/access_right/c_abf2 Reserva de todos los derechos http://rightsstatements.org/vocab/InC/1.0/ |
| eu_rights_str_mv |
openAccess |
| dc.format.none.fl_str_mv |
application/pdf application/pdf |
| dc.publisher.none.fl_str_mv |
Elsevier |
| publisher.none.fl_str_mv |
Elsevier |
| dc.source.none.fl_str_mv |
reponame:RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia instname:Universitat Politècnica de València (UPV) |
| instname_str |
Universitat Politècnica de València (UPV) |
| reponame_str |
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia |
| collection |
RiuNet. Repositorio Institucional de la Universitat Politécnica de Valéncia |
| repository.name.fl_str_mv |
|
| repository.mail.fl_str_mv |
|
| _version_ |
1869407447785930752 |
| score |
15,301603 |