Effect of the Pt–Pd molar ratio in bimetallic catalysts supported on sulfated zirconia on the gas-phase hydrodechlorination of chloromethanes
Bimetallic Pt:Pd catalysts with different molar ratios and 0.5 wt.% overall metal load supported on sulfated zirconia catalysts were synthesized and tested in the gas-phase hydrodechlorination (HDC) of chloromethanes and their mixtures. The catalysts were characterized by adsorption–desorption of N...
| Autores: | , , , , , , , |
|---|---|
| Tipo de recurso: | artículo |
| Estado: | Versión aceptada para publicación |
| Fecha de publicación: | 2017 |
| País: | España |
| Institución: | Consejo Superior de Investigaciones Científicas (CSIC) |
| Repositorio: | DIGITAL.CSIC. Repositorio Institucional del CSIC |
| OAI Identifier: | oai:digital.csic.es:10261/182802 |
| Acceso en línea: | http://hdl.handle.net/10261/182802 |
| Access Level: | acceso abierto |
| Palabra clave: | Chloromethanes Hydrodechlorination Palladium Platinum Sulfated zirconia |
| Sumario: | Bimetallic Pt:Pd catalysts with different molar ratios and 0.5 wt.% overall metal load supported on sulfated zirconia catalysts were synthesized and tested in the gas-phase hydrodechlorination (HDC) of chloromethanes and their mixtures. The catalysts were characterized by adsorption–desorption of N at −196 °C, X-ray diffraction, X-ray photoelectronic spectroscopy, temperature-programmed reduction, and aberration-corrected scanning transmission electron microscopy (STEM). The effect of the Pt:Pd molar ratio on the activity, stability, and selectivity was analyzed. The high acidity of the sulfated zirconia results in metal particles of small size (mainly <5 nm), as confirmed by STEM. The bimetallic catalysts showed higher stability than the monometallic ones, as demonstrated in long-term experiments (80 h on stream), confirming the positive effect of combining the two metallic phases. Turnover frequency (TOF) values in the range 0.0007–0.0168 s and apparent activation energies between ≈41 and 44 kJ·mol were obtained. TOF values for dichloromethane HDC increased with increasing mean metal particle size within the range of this work (≈1.2–2.3 nm). The catalysts with Pt:Pd molar ratios of 1:3 and 1:1 showed significantly better performance than the 3:1 one for overall dechlorination due to their higher atomic metal content and TOF at the same total metal weight load (0.5%). |
|---|