Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping
La and Nb codoping of ferroelectric five-layer Aurivillius phase Sr2Bi4Ti5O18 ( ∼ 560 K), induces compositional disorder and diffuse relaxor transitions at much lower temperatures than the parent compound, while preserving the orthorhombic structure. For moderate La and Nb concentrations, the erroel...
| Autores: | , , , |
|---|---|
| Tipo de recurso: | artículo |
| Estado: | Versión publicada |
| Fecha de publicación: | 2024 |
| País: | España |
| Institución: | Universidad de Zaragoza |
| Repositorio: | Zaguán. Repositorio Digital de la Universidad de Zaragoza |
| OAI Identifier: | oai:zaguan.unizar.es:132430 |
| Acceso en línea: | http://zaguan.unizar.es/record/132430 |
| Access Level: | acceso abierto |
| id |
ES_25ebd61b1f4e65ec0fa6fac6529091a5 |
|---|---|
| oai_identifier_str |
oai:zaguan.unizar.es:132430 |
| network_acronym_str |
ES |
| network_name_str |
España |
| repository_id_str |
|
| spelling |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codopingLafuerza, SaraGracia, DavidBlasco, JavierEvangelisti, MarcoLa and Nb codoping of ferroelectric five-layer Aurivillius phase Sr2Bi4Ti5O18 ( ∼ 560 K), induces compositional disorder and diffuse relaxor transitions at much lower temperatures than the parent compound, while preserving the orthorhombic structure. For moderate La and Nb concentrations, the erroelectric properties are enhanced in the vicinity of room temperature, and so is the electrocaloric effect as measured directly with a homemade quasi-adiabatic calorimeter. The adiabatic temperature change reaches, e.g., in Sr2Bi3.44La0.5Ti4.8Nb0.2O18, ⁓ 0.3 K at 355 K with a temperature span ⁓ 15 K, under = 37 kV/cm. Besides, a large field dispersion of the electrocaloric effect is found, ascribed to field-induced transitions from short-range-ordered relaxor to long-range-ordered ferroelectric states. Indirect estimations of the electrocaloric effect from electric polarization data are not able to quantitatively predict the direct results and emphasize the need of applying direct measurement methods, especially for relaxor ferroelectrics.2024info:eu-repo/semantics/articleinfo:eu-repo/semantics/publishedVersionapplication/pdfhttp://zaguan.unizar.es/record/132430reponame:Zaguán. Repositorio Digital de la Universidad de Zaragozainstname:Universidad de ZaragozaInglésinfo:eu-repo/grantAgreement/ES/DGA/E11-23Rinfo:eu-repo/grantAgreement/EC/H2020/101029019This project has received funding from the European Union’s Horizon 2020 research and innovation program under grant agreement No H2020 101029019-EAGERinfo:eu-repo/grantAgreement/ES/MICINN/PID2021-124734OB-C21info:eu-repo/semantics/openAccessoai:zaguan.unizar.es:1324302026-05-29T13:59:51Z |
| dc.title.none.fl_str_mv |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping |
| title |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping |
| spellingShingle |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping Lafuerza, Sara |
| title_short |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping |
| title_full |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping |
| title_fullStr |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping |
| title_full_unstemmed |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping |
| title_sort |
Electrocaloric effect near room temperature in lead-free Aurivillius phase Sr2Bi4Ti5O18 upon La and Nb codoping |
| dc.creator.none.fl_str_mv |
Lafuerza, Sara Gracia, David Blasco, Javier Evangelisti, Marco |
| author |
Lafuerza, Sara |
| author_facet |
Lafuerza, Sara Gracia, David Blasco, Javier Evangelisti, Marco |
| author_role |
author |
| author2 |
Gracia, David Blasco, Javier Evangelisti, Marco |
| author2_role |
author author author |
| description |
La and Nb codoping of ferroelectric five-layer Aurivillius phase Sr2Bi4Ti5O18 ( ∼ 560 K), induces compositional disorder and diffuse relaxor transitions at much lower temperatures than the parent compound, while preserving the orthorhombic structure. For moderate La and Nb concentrations, the erroelectric properties are enhanced in the vicinity of room temperature, and so is the electrocaloric effect as measured directly with a homemade quasi-adiabatic calorimeter. The adiabatic temperature change reaches, e.g., in Sr2Bi3.44La0.5Ti4.8Nb0.2O18, ⁓ 0.3 K at 355 K with a temperature span ⁓ 15 K, under = 37 kV/cm. Besides, a large field dispersion of the electrocaloric effect is found, ascribed to field-induced transitions from short-range-ordered relaxor to long-range-ordered ferroelectric states. Indirect estimations of the electrocaloric effect from electric polarization data are not able to quantitatively predict the direct results and emphasize the need of applying direct measurement methods, especially for relaxor ferroelectrics. |
| publishDate |
2024 |
| dc.date.none.fl_str_mv |
2024 |
| dc.type.none.fl_str_mv |
info:eu-repo/semantics/article info:eu-repo/semantics/publishedVersion |
| format |
article |
| status_str |
publishedVersion |
| dc.identifier.none.fl_str_mv |
http://zaguan.unizar.es/record/132430 |
| url |
http://zaguan.unizar.es/record/132430 |
| dc.language.none.fl_str_mv |
Inglés |
| language_invalid_str_mv |
Inglés |
| dc.relation.none.fl_str_mv |
info:eu-repo/grantAgreement/ES/DGA/E11-23R info:eu-repo/grantAgreement/EC/H2020/101029019 This project has received funding from the European Union’s Horizon 2020 research and innovation program under grant agreement No H2020 101029019-EAGER info:eu-repo/grantAgreement/ES/MICINN/PID2021-124734OB-C21 |
| dc.rights.none.fl_str_mv |
info:eu-repo/semantics/openAccess |
| eu_rights_str_mv |
openAccess |
| dc.format.none.fl_str_mv |
application/pdf |
| dc.publisher.none.fl_str_mv |
|
| publisher.none.fl_str_mv |
|
| dc.source.none.fl_str_mv |
reponame:Zaguán. Repositorio Digital de la Universidad de Zaragoza instname:Universidad de Zaragoza |
| instname_str |
Universidad de Zaragoza |
| reponame_str |
Zaguán. Repositorio Digital de la Universidad de Zaragoza |
| collection |
Zaguán. Repositorio Digital de la Universidad de Zaragoza |
| repository.name.fl_str_mv |
|
| repository.mail.fl_str_mv |
|
| _version_ |
1869404790940762112 |
| score |
15,300724 |