Influence of ECAP process on mechanical, corrosion and bacterial properties of Zn-2Ag alloy for wound closure devices
Actual polymeric wound closure devices are not optimal for load-bearing applications due to the low mechanical properties and the risk of inflammation and bacterial infection mainly produced by multifil-ament and braided configurations. Biodegradable metallic Zn alloys are promising materials candid...
| Autores: | , , , , , , , |
|---|---|
| Tipo de recurso: | artículo |
| Estado: | Versión publicada |
| Fecha de publicación: | 2023 |
| País: | España |
| Institución: | Fundació Sant Joan de Déu |
| Repositorio: | r-FSJD. Repositorio Institucional de Producción Científica de la Fundació Sant Joan de Déu |
| OAI Identifier: | oai:fsjd.fundanetsuite.com:p24664 |
| Acceso en línea: | https://fsjd.fundanetsuite.com/Publicaciones/ProdCientif/PublicacionFrw.aspx?id=24664 |
| Access Level: | acceso abierto |
| Palabra clave: | Binary alloys Biomaterials Equal channel angular pressing Nanoindentation Ultrafine-grained materials Zinc alloys |
| Sumario: | Actual polymeric wound closure devices are not optimal for load-bearing applications due to the low mechanical properties and the risk of inflammation and bacterial infection mainly produced by multifil-ament and braided configurations. Biodegradable metallic Zn alloys are promising materials candidates; however, mechanical performance, corrosion behaviour, and biological response should be controlled in order to inhibit the risk of inflammation and bacterial infection. To this end, a Zn-2Ag (2 wt% Ag) alloy was processed by ECAP to evaluate the concurrent combined effect of grain refinement and Ag alloying on biodegradation and antibacterial activity. Two ECAP cycles were successfully applied to a Zn-2Ag alloy obtaining a homogeneous ultra-fine-grained structure in which nanoindentation maps suggested isotro-pic mechanical properties. Lower UTS and YS with higher elongation was reported after ECAP with similar corrosion rates as before processing. ECAP processed samples showed a homogeneous Ag+ release below the minimum inhibitory concentration for S. Aureus and no antibacterial effect was observed by diffusion. As expected, the presence of Ag in Zn-Ag alloys reduced bacterial attachment. Nevertheless, ECAP processed Zn-2Ag provided an excellent antibacterial activity after 3 h probably caused by the uniformly degraded and thus, non- stable, surface observed after bacterial adhesion.(c) 2023 The Authors. Published by Elsevier Ltd. This is an open access article under the CC BY-NC-ND license (http://creativecommons.org/licenses/by-nc-nd/4.0/). |
|---|