Evaluation of titanium dental implants after early failure of osseointegration by means of X-ray photoelectron spectoscopy, electron microscopy and histological studies
In this work, we analysed 56 clinically failed and retrieved implants by means of scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS) and histological studies. The surface contamination was compared to that of unused control implants and with that of the same implants after cl...
| Autores: | , , |
|---|---|
| Tipo de recurso: | artículo |
| Fecha de publicación: | 2010 |
| País: | España |
| Institución: | Varias* (Consorci de Biblioteques Universitáries de Catalunya, Centre de Serveis Científics i Acadèmics de Catalunya) |
| Repositorio: | Recercat. Dipósit de la Recerca de Catalunya |
| OAI Identifier: | oai:recercat.cat:20.500.12328/2931 |
| Acceso en línea: | http://hdl.handle.net/20.500.12328/2931 http://dx.doi.org/10.4236/jbise.2010.311139 |
| Access Level: | acceso abierto |
| Palabra clave: | Implant dental Titani Contaminació Osteointegració Implante dental Titanio Contaminación Osteointegración Dental implants Titanium Contamination Osseointegration 616.3 |
| Sumario: | In this work, we analysed 56 clinically failed and retrieved implants by means of scanning electron microscopy (SEM), X-ray photoelectron spectroscopy (XPS) and histological studies. The surface contamination was compared to that of unused control implants and with that of the same implants after cleaning in a basic medium. The surfaces of the unused implants presented considerable contamination. In particular, high levels of carbon were detected. The nature of this C was elucidated by XPS analysis of the lubricant used in the machining process. The same contamination was observed in the retrieved implants. Histological studies were carried out by means of light microscopy. Fibrosis and granulomatous lesions were detected in the tissues. XPS analysis indicated the presence of traces of other elements (Na, Ca, Zn, S, F, etc.) that were not related to impurities in cpTi. We examined a cleaning process in a basic medium that eliminates the organic components of the implant surfaces. The cleaned implants were implanted in the patients and the results were excellent. None of the implants failed in following 7 months. |
|---|