Sugar cane bagasse ash as a pozzolanic material
This study aimed to verify the SCBA's potential use as a partial replacement of Portland cement. Therefore, the experiment was divided in two stages; in the first, mineralogical and chemical analyses were performed with two samples of ash, in-natura and calcined at a temperature of 600°C for 6h...
| Autores: | , , , |
|---|---|
| Tipo de recurso: | artículo |
| Estado: | Versión publicada |
| Fecha de publicación: | 2017 |
| País: | Colombia |
| Institución: | Universidad Nacional de Colombia |
| Repositorio: | Repositorio UN |
| Idioma: | español |
| OAI Identifier: | oai:repositorio.unal.edu.co:unal/60411 |
| Acceso en línea: | https://repositorio.unal.edu.co/handle/unal/60411 http://bdigital.unal.edu.co/58743/ |
| Access Level: | acceso abierto |
| Palabra clave: | 62 Ingeniería y operaciones afines / Engineering Sugar cane bagasse ash pozzolanic activity mechanical performance ceniza de bagazo de caña de azúcar actividad puzolánica comportamiento mecánico |
| Sumario: | This study aimed to verify the SCBA's potential use as a partial replacement of Portland cement. Therefore, the experiment was divided in two stages; in the first, mineralogical and chemical analyses were performed with two samples of ash, in-natura and calcined at a temperature of 600°C for 6h. After these analyzes, it was observed that the calcined ash presented a greater tendency of material in the amorphous state, which possibly made the material the most reactive. For this reason, only the calcined ash was ground for 1 and 2h. These samples were further studied in order to check the pozzolanic activity index and the compressive strength, evaluating the replacement of 10, 20 and 30% Portland cement by ground SCBA. The results showed an increase in the pozzolanic activity index only in samples of calcined and ground SCBA, showing that calcined ash must undergo a grinding process to present pozzolanic activity. |
|---|