Influence of the Addition of Al2O3 Nanoparticles and the Duration of Pressing on the Physical Properties of OSB Panels

For greater durability, materials must withstand contact with water, making it difficult for biodegrading agents to attack. The present study produced and evaluated the heat transfer for two pressing times and the physical properties of OSB panels, produced with pinewood strands and Al2O3 nanopartic...

Descripción completa

Detalles Bibliográficos
Autores: Lima, Felipe O. [UNESP], Silva, Luana Cristal L. [UNESP], Ferreira, Bruno S. [UNESP], de Morais, César Augusto G. [UNESP], Bertolini, Marília da S. [UNESP], Barreiros, Ricardo M. [UNESP], Azambuja, Maximiliano Dos A. [UNESP], Caraschi, José Claudio [UNESP], Favarim, Higor R. [UNESP], Campos, Cristiane I. [UNESP]
Tipo de recurso: artículo
Estado:Versión publicada
Fecha de publicación:2022
País:Brasil
Institución:Universidade Estadual Paulista (UNESP)
Repositorio:Repositório Institucional da UNESP
Idioma:inglés
OAI Identifier:oai:repositorio.unesp.br:11449/241602
Acceso en línea:http://dx.doi.org/10.15376/biores.17.2.3014-3024
http://hdl.handle.net/11449/241602
Access Level:acceso abierto
Palabra clave:Heat transfer
Nanotechnology
Oriented strand board
Thickness swelling
Wood
Descripción
Sumario:For greater durability, materials must withstand contact with water, making it difficult for biodegrading agents to attack. The present study produced and evaluated the heat transfer for two pressing times and the physical properties of OSB panels, produced with pinewood strands and Al2O3 nanoparticles addition. The nanoparticles were synthesized through the sol-gel-protein method and added to the resin in the proportion of 0.5%. During the pressing process, heat transfer and distribution in the central region of the particle mat were evaluated using a type K thermocouple. After its fabrication, the panels were characterized to evaluate density, moisture content, thickness swelling, and water absorption. The results obtained indicated that the nanoparticle addition caused a refractory effect in the central region of the mat, leading to a small reduction in the pressing temperature for the 600 s cycle. However, there was no compromise in resin cure, indicating good interaction of the panels with nanoparticles in water contact, for both pressing times. There was an improvement in the panel thickness swelling with the addition of 0.5% of Al2O3 nanoparticles, with all properties meeting the Class 1 indicators of the EN 300 (2006) standard.