ABSTRACT Nanoparticles of TiO2 have been the main semiconductor applied in Dye-sensitized solar cells (DSSCs). In this work, solar cells were developed from the electrophoretic deposition of anatase titanium dioxide (TiO2) films on conductive glasses. The electrophoretic deposition was perfomed with...

Descripción completa

Detalles Bibliográficos
Autores: Souza,Antonio Paulo Santos, Cavalcante,Natália Macêdo, Freire,Francisco Nivaldo Aguiar, Almeida,Ana Fabíola Leite
Tipo de recurso: artículo
Estado:Versión publicada
Fecha de publicación:2021
País:Brasil
Institución:Matéria (Rio de Janeiro. Online)
Repositorio:Matéria (Rio de Janeiro. Online)
Idioma:inglés
OAI Identifier:oai:scielo:S1517-70762021000100338
Acceso en línea:http://old.scielo.br/scielo.php?script=sci_arttext&pid=S1517-70762021000100338
Access Level:acceso abierto
Palabra clave:Dye-sensitized solar cells
Electrophoresis
Titanium dioxide
Film
Mesoporous. Photoanode
Descripción
Sumario:ABSTRACT Nanoparticles of TiO2 have been the main semiconductor applied in Dye-sensitized solar cells (DSSCs). In this work, solar cells were developed from the electrophoretic deposition of anatase titanium dioxide (TiO2) films on conductive glasses. The electrophoretic deposition was perfomed with a constant voltage of 80V for 2 minutes and, after drying, the films were sintered at three different temperatures: 450 °C, 550 °C and 600 °C. In the assembly of the cells, the titanium dioxide films were sensitized by Ruthenizer 535-bisTBA dye (N719) and an electrolyte containing the iodide / tri-iodide redox pair and a commercial transparent platinum counter electrode were used. TiO2 films were characterized by scanning electron microscopy, dispersive energy spectroscopy and X-ray diffraction and photo-electrochemical techniques. The energy conversion rates were 0.2646% for the sintered film at 450 °C, 0.1209% for the sintered film at 550 °C and 0.1137% for the film sintered at 600 °C.