Localized mechanics of dentin self-etching adhesive system

The bond strength of composite resins (CRs) to dentin is influenced by the interfacial microstructure of the hybrid layer (HL) and the resin tags (TAG). The contemporary self-etching primer adhesive systems overcame the inconvenient of the etch-and-rinse protocol. Studies, however, have demonstrated...

Descripción completa

Detalles Bibliográficos
Autores: Anchieta, Rodolfo Bruniera [UNESP], Rocha, Eduardo Passos [UNESP], Ko, Ching-Chang, Sundfeld, Renato Herman [UNESP], Martin, Manoel [UNESP], Archangelo, Carlos Marcelo [UNESP]
Tipo de recurso: artículo
Estado:Versión publicada
Fecha de publicación:2007
País:Brasil
Institución:Universidade Estadual Paulista (UNESP)
Repositorio:Repositório Institucional da UNESP
Idioma:inglés
OAI Identifier:oai:repositorio.unesp.br:11449/34317
Acceso en línea:http://dx.doi.org/10.1590/S1678-77572007000400015
http://hdl.handle.net/11449/34317
Access Level:acceso abierto
Palabra clave:dentin-bonding agents
finite element analysis
dentin
dental acid etching
Descripción
Sumario:The bond strength of composite resins (CRs) to dentin is influenced by the interfacial microstructure of the hybrid layer (HL) and the resin tags (TAG). The contemporary self-etching primer adhesive systems overcame the inconvenient of the etch-and-rinse protocol. Studies, however, have demonstrated that HL thickness and TAG length vary according to the wetting time and additional use of acid-etching prior to self-etching primers. This study investigated the localized stress distribution in the HL and the dentin/adhesive interface. Two HL thicknesses (3 or 6 mu m), two TAG lengths (13 or 17 mu m) and two loading conditions (perpendicular and oblique-25 degrees) were investigated by the finite element (FE) analysis. Five two-dimensional FE models (M) of a dentin specimen restored with CR (38 x 64 mu m) were constructed: M1 - no HL and no TAG; M2 - 3 mu m of HL and 13 mu m of TAG; M3 - 3 mu m of HL and 17 mu m of TAG; M4 - 6 mu m of HL and 13 mu m of TAG; and M5 - 6 mu m of HL and 17 mu m of TAG. Two distributed loadings (L) (20N) were applied on CR surface: L1 - perpendicular, and L2 - oblique (25 degrees). Fixed interfacial conditions were assigned on the border of the dentin specimen. Ansys 10.0 (Ansys (R), Houston, PA, USA) software was used to calculate the stress fields. The peak of von Mises (sigma(vM)) and maximum principal stress (sigma(max)) was higher in L2 than in L1. Microstructures (HL and TAG) had no effect on local stresses for L1. Decreasing HL decreased sigma(vM) and sigma(max) in all structures for L2, but the TAG length had influence only on the peributular dentin. The thickness of HL had more influence on the sigma(vM) and sigma(max) than TAG length. The peritubular dentin and its adjacent structures showed the highest sigma(vM) and sigma(max), mainly in the oblique loading.