Physical evaluation of the luting systems for veneer ceramic after aging / Avaliação física dos sistemas de cimentação para faceta cerâmica após envelhecimento

The aim of this in vitro study was evaluated the amount of color change and degree of conversion of the luting systems for ceramic veneer cementation. Forty-eight human incisors were randomly divided into six groups (n=8) according to the bonding procedure: RelyX Veneer/Single Bond 2; RelyX ARC/Sing...

Descripción completa

Detalles Bibliográficos
Autores: Prieto, Lucia Trazzi, Araújo, Cíntia Tereza de Pimenta, de Oliveira, Dayane Carvalho Ramos Salles, Coppini, Erick Kamiya, Pierote, Josué Junior Araujo, Câmara, João Victor Frazão, Pereira, Gisele Damiana da Silveira, Barbosa, Isabel Ferreira, Tinoco, Justine Monteiro Monnerat, Vianna, Renato Feres de Carvalho, Fried, Hana, Dias, Carlos Tadeu Santos, Paulillo, Luis Alexandre Maffei Sartini
Tipo de recurso: artículo
Estado:Versión publicada
Fecha de publicación:2022
País:Brasil
Institución:Instituto Superior de Educação Vera Cruz (VeraCruz)
Repositorio:Revista Veras
Idioma:inglés
OAI Identifier:oai:ojs2.ojs.brazilianjournals.com.br:article/47534
Acceso en línea:https://ojs.brazilianjournals.com.br/ojs/index.php/BRJD/article/view/47534
Access Level:acceso abierto
Palabra clave:color
dental veneers
aging
resin cements.
Descripción
Sumario:The aim of this in vitro study was evaluated the amount of color change and degree of conversion of the luting systems for ceramic veneer cementation. Forty-eight human incisors were randomly divided into six groups (n=8) according to the bonding procedure: RelyX Veneer/Single Bond 2; RelyX ARC/Single Bond 2; Filtek Z350 XT Flowable /Single Bond 2; Variolink Veneer/Tetric N-Bond; Variolink II/Tetric N-Bond; Tetric N-Flow/Tetric N-Bond. Ceramic veneers (IPS Empress Esthetic) were cemented using the different bonding procedures. Color differences of the ceramic surface after cementation and 300 h(150kJ/m2) of UV aging test, were examined with a colorimeter. Fourier transform infrared spectroscopy (FT-IR) was used to evaluate the degree of conversion for each luting system. Data were analyzed with one-way ANOVA and Tukey's test (α=0.05). All the luting systems demonstrated significant changes in color stability. The ΔE of the systems ranged from 6,11 to 9,33. Tetric N-Flow and RelyX Veneer showed the highest degree of conversion, while lowest values were found for RelyX ARC. All luting systems demonstrated clinically unacceptable (ΔE≥ 3.3) color changes. Despite to the dual cure of the RelyX ARC luting cement, it showed the lowest degree of conversion values, while Tetric N-Flow and RelyX Veneer presented the highest and similar degree of conversion.