USE OF LINEAR ALKYLBENZENE SULFONATE (LAS) AND POLYCARBOXYLATE-ETHER (PCE) AS REAGENTS IN IRON ORE FLOTATION

Flotation is one of the separation techniques that has been used by the mineral industry and its importance has increased due to its better performance in the concentration of low grade ores. Specific chemical reagents are used in flotation in order to promote the hydrophobicity control of minerals...

Descripción completa

Detalles Bibliográficos
Autores: Carvalho, José Maria Franco, Vasconcelos, Mariane Batista Oliveira, Moreira, Luanne Phâmella Henriques, Mendes, Julia Castro, Pereira, Carlos Alberto
Tipo de recurso: artículo
Estado:Versión publicada
Fecha de publicación:2017
País:Brasil
Institución:Instituto Federal do Rio Grande do Norte (IFRN)
Repositorio:Holos
Idioma:inglés
OAI Identifier:oai:holos.ifrn.edu.br:article/6374
Acceso en línea:http://www2.ifrn.edu.br/ojs/index.php/HOLOS/article/view/6374
Access Level:acceso abierto
Palabra clave:Flotation reagents
iron ore flotation
microflotation test
Yates algorithm
Descripción
Sumario:Flotation is one of the separation techniques that has been used by the mineral industry and its importance has increased due to its better performance in the concentration of low grade ores. Specific chemical reagents are used in flotation in order to promote the hydrophobicity control of minerals dispersed in a pulp, among them, surfactants have been studied with good results. In this study, a substance based on Linear Alkylbenzene Solfonate (LAS), and a concrete admixture based on Policarboxilate-ether (PCE) were tested as reagents in iron ore flotation. The tests were performed in a friable hematite sample, using the microflotation technique. The Yates complete replicated factorial method for three variables and two levels was used in experimental planning. The variables evaluated was pH (9-11); LAS content (1000-5000 g/cm³); and PCE content (100-1000 g/cm³). The best result (84.1% floated) was obtained for combination pH=9, LAS content = 5000 g/cm³ and PCE content = 100 g/cm³