Structural Characterization and Thermoelectric Properties of Br-Doped AgSnm[Sb0.8Bi0.2]Te2+m Systems
Herein, we report the synthesis, structural and microstructural characterization, and thermoelectric properties of AgSnm[Sb0.8Bi0.2]Te2+m and Br-doped telluride systems. These compounds were prepared by solid-state reaction at high temperature. Powder X-ray diffraction data reveal that these samples...
| Authors: | , , , , , , |
|---|---|
| Format: | article |
| Publication Date: | 2023 |
| Country: | España |
| Institution: | Universidad Complutense de Madrid (UCM) |
| Repository: | Docta Complutense |
| Language: | English |
| OAI Identifier: | oai:docta.ucm.es:20.500.14352/103523 |
| Online Access: | https://hdl.handle.net/20.500.14352/103523 |
| Access Level: | Open access |
| Keyword: | 546 Tellurides Seebeck coefficient Thermal conductivity Lead-free thermoelectric materials Performance SnTe Thermopower Power Química inorgánica (Química) 2303 Química Inorgánica |
| Summary: | Herein, we report the synthesis, structural and microstructural characterization, and thermoelectric properties of AgSnm[Sb0.8Bi0.2]Te2+m and Br-doped telluride systems. These compounds were prepared by solid-state reaction at high temperature. Powder X-ray diffraction data reveal that these samples exhibit crystal structures related to the NaCl-type lattice. The microstructures and morphologies are investigated by scanning electron microscopy, energy-dispersive X-ray spectroscopy (EDS), and high-resolution transmission electron microscopy (HRTEM). Positive values of the Seebeck coefficient (S) indicate that the transport properties are dominated by holes. The S of undoped AgSnm[Sb0.8Bi0.2]Te2+m ranges from +40 to 57 mu V.K-1. Br-doped samples with m = 2 show S values of +74 mu V.K-1 at RT, and the Seebeck coefficient increases almost linearly with increasing temperature. The total thermal conductivity (kappa(tot)) monotonically increases with increasing temperature (10-300 K). The ktot values of undoped AgSnm[Sb0.8Bi0.2]Te2+m are similar to 1.8 W m(-1) K-1 (m = 4) and similar to 1.0 W m(-1) K-1 (m = 2) at 300 K. The electrical conductivity (sigma) decreases almost linearly with increasing temperature, indicating metal-like behavior. The ZT value increases as a function of temperature. A maximum ZT value of similar to 0.07 is achieved at room temperature for the Br-doped phase with m = 4. |
|---|