Effect of the Nd:YAG laser on sealer penetration into root canal surfaces: a confocal microscope analysis
Objectives: The objective of this in vitro study was to evaluate the use of the Neodymium:Yttrium-Aluminium-Garnet (Nd:YAG) laser as part of the root canal treatment on the penetration of sealer into dentinal tubules. Methods: Eighty extracted lower premolars were randomly assigned to two groups (n...
| Autores: | , , , , , |
|---|---|
| Formato: | artículo |
| Estado: | Versión aceptada para publicación |
| Fecha de publicación: | 2014 |
| País: | España |
| Recursos: | Universidad de Sevilla (US) |
| Repositorio: | idUS. Depósito de Investigación de la Universidad de Sevilla |
| OAI Identifier: | oai:idus.us.es:11441/106217 |
| Acesso em linha: | https://hdl.handle.net/11441/106217 |
| Access Level: | acceso abierto |
| Palavra-chave: | Confocal microscope Nd:YAG laser Endodontic instrumentation Dentinal permeability Endodontic sealer Sealer penetration |
| Resumo: | Objectives: The objective of this in vitro study was to evaluate the use of the Neodymium:Yttrium-Aluminium-Garnet (Nd:YAG) laser as part of the root canal treatment on the penetration of sealer into dentinal tubules. Methods: Eighty extracted lower premolars were randomly assigned to two groups (n = 40 each): Control group (CG), subjected to a conventional protocol of endodontic instrumentation and obturation; and Laser group (LG), in which Nd:YAG laser irradiations were combined with conventional preparation and obturation. Endodonted samples were sectioned at 3 and 5 mm from the apex and observed under a confocal scanning microscope (CLSM). The penetration depth into the dentinal tubules and the extension of the intracanal perimeter infiltrated by sealer were measured. The Student-Newman Keuls test was run for between-group comparisons (α=.05). Results: The depth of sealer penetration into dentinal tubules did not differ among groups. LG samples showed the significantly highest percentage of penetrated perimeter at 3 mm from the root apex. Within each group, the greatest depth of penetration (P=.0001), and the major percentage of penetrated perimeter (P <.001), were recorded at 5 mm. Conclusions: The application of the Nd:YAG laser after instrumentation did not improve the depth of sealer penetration into the dentinal tubules. The laser enlarged the total penetrable perimeter near the apex |
|---|