Influence of sodium silicate modulus on iron ore flotation with sodium oleate.
This paper presents the influence of sodium silicate modulus on iron ore flotation with sodium oleate collector. Bench flotation tests were performed at pH 7 with actual iron ore from Quadrilátero Ferrífero, Brazil, with 42.8% Fe and 37.2% SiO2. Iron recovery averaged above 90% and the Fe contents i...
| Autores: | , |
|---|---|
| Tipo de recurso: | artículo |
| Estado: | Versión publicada |
| Fecha de publicación: | 2013 |
| País: | Brasil |
| Institución: | Universidade Federal de Ouro Preto (UFOP) |
| Repositorio: | Repositório Institucional da UFOP |
| Idioma: | inglés |
| OAI Identifier: | oai:repositorio.ufop.br:123456789/5223 |
| Acceso en línea: | http://www.repositorio.ufop.br/handle/123456789/5223 https://doi.org/10.1016/j.minpro.2013.09.002 |
| Access Level: | acceso abierto |
| Palabra clave: | Iron ore Sodium silicate modulus Sodium oleate Flotation |
| Sumario: | This paper presents the influence of sodium silicate modulus on iron ore flotation with sodium oleate collector. Bench flotation tests were performed at pH 7 with actual iron ore from Quadrilátero Ferrífero, Brazil, with 42.8% Fe and 37.2% SiO2. Iron recovery averaged above 90% and the Fe contents in the concentrate were above 55%. The highest values of Fe grade and lowest of SiO2were obtainedwith lowlevels of pulp density and sodium silicate dosage and with high level of sodiumoleate. Increase of sodiumsilicate modulus had a small influence on response variables. |
|---|